HAZ and Structural Defects Control in Key-Hole Welding of Titanium Using a Reptitively-Pulsed Nd: Yag Laser
DOI
-
Abstract
HAZ, porosity and cracks were investigated when welding 0.9 mm thick titanium sheets using a 10 J pulsed Nd: Yag laser. The effects of welding speed, joints fit-up, shielding gas, and laser parameters are presented. For optimum welding quality, 0.25 m/min scanning speed, 10 \ell/min gas flow rate and 72 Watt average power were used. Welds of narrow heat affected zone (HAZ) with small level of porosity were obtained.